We generally continually give you quite possibly the most conscientious shopper company, and the widest variety of designs and styles with finest materials. These endeavours include the availability of customized designs with speed and dispatch for Lignosulfonic Acid Sodium Salt, Admixture To Increase Workability Of Concrete, Lignosulfonic Acid/Sodium Salt, Our final target is "To consider the most effective, To be the Best". Please experience cost-free to call with us if you have any prerequisites.
2021 High quality Sodium Naphthalene Sulfonate Formaldehyde - CL-SNF-18 – Chengli Detail:

Detection project

Performance index Measured value

Water reducing ratio %

≥14

≥20

Bleeding rate ratio %

≤90

≤80

Gas content %

≤3.0

≤2.0

The gap of condense time (min)

Initial condense

-90~120

-90~120

Final condense

Ratio of compressive strength %

1d

≥140

≥160

3d

≥130

≥150

7d

≥125

≥140

28d

≥120

≥130

Ratio of shrinkage rate %

≤135

≤135

Corrosion effect for steel

None

None

Uniformity index

Detection project

snf Powder Index(SNF-C)

Solid content (%)

≥92

Fitness (%)

0.315mm (residue)<10

PH value(10g/L)

7–9

Chlorine ion content(%)

≤0.5

Sodium sulfate content(%)

≤18

Total alkali content(%)

≤20

Insoluble matter(%)

≤0.5

Cement net fluidity(mm)

≥220

Appearance

Yellowish-brown powder

Widely used in concrete engineering, prefabricated, sleeper, bridges, tunnels, national defense, military engineering, water conservancy, power engineering, port terminals, airport runway, high-rise building engineering.

Dosage: 0.5%-1.5%, the user should according to the need to experiment to determine the optimal dosage.

Remarkable Plasticity: Statistically, compression strength on the 1stday, the 3rd day and 28th day after single application is increased by 60%-90% and 25%-60% respectively when it is added at standard blend dosage. As the result, compression strength, tensile strength, buckling strength and modulus of elasticity will be improved to some extent.

Under the condition of same water/cement ratio, collapsibility can be increased 5-8 times when it is added at 0.75% blend dosage.

15-20% of cement can be reserved when the agent is blended at 0.75% blend dosage, which is preconditioned by same collapsibility and strength.


Product detail pictures:

2021 High quality Sodium Naphthalene Sulfonate Formaldehyde - CL-SNF-18 – Chengli detail pictures


Related Product Guide:

It is actually our accountability to satisfy your needs and effectively serve you. Your pleasure is our best reward. We're on the lookout forward for your stop by for joint growth for 2021 High quality Sodium Naphthalene Sulfonate Formaldehyde - CL-SNF-18 – Chengli , The product will supply to all over the world, such as: Iran, Hanover, Philadelphia, We follow up the career and aspiration of our elder generation, and we are eager to open up a new prospect in this field, We insist on "Integrity, Profession, Win-win Cooperation", because we have a strong backup, that are excellent partners with advanced manufacturing lines, abundant technical strength, standard inspection system and good production capacity.
  • This is a reputable company, they have a high level of business management, good quality product and service, every cooperation is assured and delighted!
    5 Stars By Riva from Los Angeles - 2018.06.30 17:29
    The accounts manager made a detailed introduction about the product, so that we have a comprehensive understanding of the product, and ultimately we decided to cooperate.
    5 Stars By Myra from Montreal - 2017.03.28 12:22
    Write your message here and send it to us