It adheres on the tenet "Honest, industrious, enterprising, innovative" to acquire new solutions regularly. It regards shoppers, success as its very own success. Let us establish prosperous future hand in hand for Concrete Retarder, Admixture Concrete, Precast Admixtures, Our final target is "To consider the most effective, To be the Best". Please experience cost-free to call with us if you have any prerequisites.
Best quality Sodium Naphthalene Sulfonate Formaldehyde Condensate - CL-SNF-5 – Chengli Detail:

Detection project

Performance index Measured value

Water reducing ratio %

≥14

≥20

Bleeding rate ratio %

≤90

≤80

Gas content %

≤3.0

≤2.0

The gap of condense time (min)

Initial condense

-90~120

-90~120

Final condense

Ratio of compressive strength %

1d

≥140

≥160

3d

≥130

≥150

7d

≥125

≥140

28d

≥120

≥130

Ratio of shrinkage rate %

≤135

≤135

Corrosion effect for steel

None

None

Uniformity index

Detection project

snf Powder Index

Solid content (%)

≥92

Fitness (%)

0.315mm (residue)<10

PH value(10g/L)

7–9

Chlorine ion content(%)

≤0.5

Sodium sulfate content(%)

≤5

Total alkali content(%)

≤20

Insoluble matter(%)

≤0.5

Cement net fluidity(mm)

≥220

Appearance

Yellowish-brown powder

Widely used in concrete engineering, prefabricated, sleeper, bridges, tunnels, national defense, military engineering, water conservancy, power engineering, port terminals, airport runway, high-rise building engineering.

Dosage: 0.5%-0.8%, the user should according to the need to experiment to determine the optimal dosage.

Remarkable Plasticity: Statistically, compression strength on the 1stday, the 3rd day and 28th day after single application is increased by 60%-90% and 25%-60% respectively when it is added at standard blend dosage. As the result, compression strength, tensile strength, buckling strength and modulus of elasticity will be improved to some extent.

Under the condition of same water/cement ratio, collapsibility can be increased 5-8 times when it is added at 0.75% blend dosage.

15-20% of cement can be reserved when the agent is blended at 0.75% blend dosage, which is preconditioned by same collapsibility and strength.


Product detail pictures:

Best quality Sodium Naphthalene Sulfonate Formaldehyde Condensate - CL-SNF-5 – Chengli detail pictures


Related Product Guide:

We believe that prolonged expression partnership is really a result of top of the range, value added support, rich encounter and personal contact for Best quality Sodium Naphthalene Sulfonate Formaldehyde Condensate - CL-SNF-5 – Chengli , The product will supply to all over the world, such as: Brunei, Malta, Bahamas, We adopted technique and quality system management, based on "customer orientated, reputation first, mutual benefit, develop with joint efforts", welcome friends to communicate and cooperate from all over the world.
  • Managers are visionary, they have the idea of "mutual benefits, continuous improvement and innovation", we have a pleasant conversation and Cooperation.
    5 Stars By Kevin Ellyson from Cannes - 2018.08.12 12:27
    We are long-term partners, there is no disappointment every time, we hope to maintain this friendship later!
    5 Stars By Alexander from Nepal - 2018.10.31 10:02
    Write your message here and send it to us