With our leading technology at the same time as our spirit of innovation,mutual cooperation, benefits and development, we are going to build a prosperous future alongside one another with your esteemed enterprise for Fdn Superplasticizer, Polycarboxylate for concrete, Precast Admixtures, We focus on for making superb top quality goods to provide support for our purchasers to ascertain long-term win-win romantic relationship.
China wholesale Fdn - CL-SNF-10 – Chengli Detail:

Detection project

Performance index Measured value

Water reducing ratio %

≥14

≥20

Bleeding rate ratio %

≤90

≤80

Gas content %

≤3.0

≤2.0

The gap of condense time (min)

Initial condense

-90~120 

-90~120

Final condense

Ratio of compressive strength %

1d

≥140

≥160

3d

≥130

≥150

7d

≥125

≥140

28d

≥120

≥130

Ratio of shrinkage rate %

≤135

≤135

Corrosion effect for steel

None

None

Uniformity index

Detection project

snf Powder Index(SNF-B)

Solid content (%)

≥92

Fitness (%)

0.315mm (residue)<10

PH value(10g/L)

7–9

Chlorine ion content(%)

≤0.5

Sodium sulfate content(%)

≤10

Total alkali content(%)

≤20

Insoluble matter(%)

≤0.5

Cement net fluidity(mm)

≥220

Appearance

Yellowish-brown powder

Widely used in concrete engineering, prefabricated, sleeper, bridges, tunnels, national defense, military engineering, water conservancy, power engineering, port terminals, airport runway, high-rise building engineering.

Dosage: 0.5%-1.0%, the user should according to the need to experiment to determine the optimal dosage.

Remarkable Plasticity: Statistically, compression strength on the 1stday, the 3rdday and 28th day after single application is increased by 60%-90% and 25%-50% respectively when it is added at standard blend dosage. As the result, compression strength, tensile strength, buckling strength and modulus of elasticity will be improved to some extent.

Under the condition of same water/cement ratio, collapsibility can be increased 4-7 times when it is added at 0.75% blend dosage.

15-18% of cement can be reserved when the agent is blended at 0.75% blend dosage, which is preconditioned by same collapsibility and strength.


Product detail pictures:

China wholesale Fdn - CL-SNF-10 – Chengli detail pictures


Related Product Guide:

We keep on with our business spirit of "Quality, Performance, Innovation and Integrity". We goal to create much more worth for our customers with our rich resources, state-of-the-art machinery, experienced workers and exceptional providers for China wholesale Fdn - CL-SNF-10 – Chengli , The product will supply to all over the world, such as: European, Saudi Arabia, Hungary, We have been very responsible for all details on our customers order no matter on warranty quality, satisfied prices, quick delivery, on time communication, satisfied packing, easy payment terms, best shipment terms, after sales service etc. We provide one-stop service and best reliability to our every customers. We work hard with our customers, colleagues, workers to make a better future.
  • This manufacturers not only respected our choice and requirements, but also gave us a lot of good suggestions, ultimately, we successfully completed the procurement tasks.
    5 Stars By Gladys from UAE - 2018.12.22 12:52
    Perfect services, quality products and competitive prices, we have work many times, every time is delighted, wish continue to maintain!
    5 Stars By Agatha from Karachi - 2018.07.27 12:26
    Write your message here and send it to us