Our development depends on the advanced equipment, excellent talents and continuously strengthened technology forces for Sodium Lignosulfonate Supplier, Sodium Lignin Sulfonate, High Range Water Reducing Admixture, We're prepared to present you with the most effective ideas over the designs of the orders in a qualified way for those who need. While in the meantime, we continue to keep on producing new technologies and building new designs so as to help make you ahead from the line of this small business.
Chinese wholesale Fdn-A - CL-SNF-18 – Chengli Detail:

Detection project

Performance index Measured value

Water reducing ratio %

≥14

≥20

Bleeding rate ratio %

≤90

≤80

Gas content %

≤3.0

≤2.0

The gap of condense time (min)

Initial condense

-90~120

-90~120

Final condense

Ratio of compressive strength %

1d

≥140

≥160

3d

≥130

≥150

7d

≥125

≥140

28d

≥120

≥130

Ratio of shrinkage rate %

≤135

≤135

Corrosion effect for steel

None

None

Uniformity index

Detection project

snf Powder Index(SNF-C)

Solid content (%)

≥92

Fitness (%)

0.315mm (residue)<10

PH value(10g/L)

7–9

Chlorine ion content(%)

≤0.5

Sodium sulfate content(%)

≤18

Total alkali content(%)

≤20

Insoluble matter(%)

≤0.5

Cement net fluidity(mm)

≥220

Appearance

Yellowish-brown powder

Widely used in concrete engineering, prefabricated, sleeper, bridges, tunnels, national defense, military engineering, water conservancy, power engineering, port terminals, airport runway, high-rise building engineering.

Dosage: 0.5%-1.5%, the user should according to the need to experiment to determine the optimal dosage.

Remarkable Plasticity: Statistically, compression strength on the 1stday, the 3rd day and 28th day after single application is increased by 60%-90% and 25%-60% respectively when it is added at standard blend dosage. As the result, compression strength, tensile strength, buckling strength and modulus of elasticity will be improved to some extent.

Under the condition of same water/cement ratio, collapsibility can be increased 5-8 times when it is added at 0.75% blend dosage.

15-20% of cement can be reserved when the agent is blended at 0.75% blend dosage, which is preconditioned by same collapsibility and strength.


Product detail pictures:

Chinese wholesale Fdn-A - CL-SNF-18 – Chengli detail pictures


Related Product Guide:

Quality First,and Customer Supreme is our guideline to provide the best service to our customers.Nowadays, we are trying our best to become one of the best exporters in our field to meet customers more need for Chinese wholesale Fdn-A - CL-SNF-18 – Chengli , The product will supply to all over the world, such as: Egypt, United States, Greek, Each customer's satisfactory is our goal. We are looking for long-term cooperation with each customer. To meet this, we keep up our quality and provide extraordinary customer service. Welcome to our company, we are expecting to cooperate with you.
  • The factory workers have rich industry knowledge and operational experience, we learned a lot in working with them,we are extremely grateful that we can encount a good company has excellent wokers.
    5 Stars By Alva from Spain - 2017.10.25 15:53
    The factory technical staff not only have high level of technology, their English level is also very good, this is a great help to technology communication.
    5 Stars By Aaron from Jersey - 2018.05.15 10:52
    Write your message here and send it to us