With this motto in mind, we have become one of the most technologically innovative, cost-efficient, and price-competitive manufacturers for Early Strength Concrete Admixture, Sodium Lignosulfonate, Textile Dispersant, We are always looking forward to forming successful business relationships with new clients around the world.
Manufacturer for Snf-A - CL-SNF-5 – Chengli Detail:

Detection project

Performance index Measured value

Water reducing ratio %

≥14

≥20

Bleeding rate ratio %

≤90

≤80

Gas content %

≤3.0

≤2.0

The gap of condense time (min)

Initial condense

-90~120

-90~120

Final condense

Ratio of compressive strength %

1d

≥140

≥160

3d

≥130

≥150

7d

≥125

≥140

28d

≥120

≥130

Ratio of shrinkage rate %

≤135

≤135

Corrosion effect for steel

None

None

Uniformity index

Detection project

snf Powder Index

Solid content (%)

≥92

Fitness (%)

0.315mm (residue)<10

PH value(10g/L)

7–9

Chlorine ion content(%)

≤0.5

Sodium sulfate content(%)

≤5

Total alkali content(%)

≤20

Insoluble matter(%)

≤0.5

Cement net fluidity(mm)

≥220

Appearance

Yellowish-brown powder

Widely used in concrete engineering, prefabricated, sleeper, bridges, tunnels, national defense, military engineering, water conservancy, power engineering, port terminals, airport runway, high-rise building engineering.

Dosage: 0.5%-0.8%, the user should according to the need to experiment to determine the optimal dosage.

Remarkable Plasticity: Statistically, compression strength on the 1stday, the 3rd day and 28th day after single application is increased by 60%-90% and 25%-60% respectively when it is added at standard blend dosage. As the result, compression strength, tensile strength, buckling strength and modulus of elasticity will be improved to some extent.

Under the condition of same water/cement ratio, collapsibility can be increased 5-8 times when it is added at 0.75% blend dosage.

15-20% of cement can be reserved when the agent is blended at 0.75% blend dosage, which is preconditioned by same collapsibility and strength.


Product detail pictures:

Manufacturer for Snf-A - CL-SNF-5 – Chengli detail pictures


Related Product Guide:

Which has a positive and progressive attitude to customer's desire, our corporation constantly improves our merchandise quality to satisfy the desires of consumers and further focuses on safety, reliability, environmental demands, and innovation of Manufacturer for Snf-A - CL-SNF-5 – Chengli , The product will supply to all over the world, such as: New Delhi, Toronto, USA, We maintain long-term efforts and self-criticism, which helps us and improvement constantly. We strive to improve customer efficiency to save costs for customers. We do our best to improve the quality of product. We will not live up to the historic opportunity of the times.
  • We are old friends, the company's product quality has been always very good and this time the price is also very cheap.
    5 Stars By Lauren from Luxemburg - 2018.09.29 13:24
    The factory has advanced equipment, experienced staffs and good management level, so product quality had assurance, this cooperation is very relaxed and happy!
    5 Stars By Sally from Thailand - 2018.10.01 14:14
    Write your message here and send it to us